By waccobird
Date 12-17-2009 18:38
Edited 12-17-2009 18:41
FullMetal* inspector
Welcome to the Forum
AWS D1.1 2008 Clause 4.8.3.1 Root Face and Side Bend Specimens explains the differences of the bend tests , Clause 4.19.1.2 Guided Bend Tests gives that info or at least directs you to the applicable figure, Figure 4.13 Side Bend Specimens which shows the specimen to be 3/8" thick and gives other bits of info like 1 1/2" wide.
Good Luck