These types of die grinder are also the PREFFERED method for cleaning up weld to NDT w/ PT. Turning of the die perpendicularly to the line of the weld allows better change of a false positive indication on a pt or mt examination. Also good for cleaning up small cracks and hard to reach places. Yeah, yeah, like the part of an IRS agent where the sun don't shine, I know...