- - By QuocBKA (*) Date 04-07-2010 14:14
The WPS qualification in accordance with ASME IX  I can’t found the range of outside diameter qualified.
So how can I determine the range approval for outside diameter qualified.

Thanks,

Q.V
Parent - By js55 (*****) Date 04-07-2010 15:23
You can't find it because it doesn't exist in Section IX.
There is no diameter range for procedure qualification.
Parent - - By Mikeqc1 (****) Date 04-07-2010 23:08
Weld metal deposited.
Parent - - By 3.2 Inspector (***) Date 04-09-2010 17:48
Kindly explain how weld metal deposited relates to diameter.
Which part of ASME sec 9 did I miss?

3.2
Parent - - By Shane Feder (****) Date 04-10-2010 00:25
3.2,
Take the outside diameter and subtract the inside diameter.
Divide by two and voila - weld metal deposited.
Hope that helps. LOL !!
Cheers,
Shane
Parent - By 3.2 Inspector (***) Date 04-10-2010 01:56
Aaahhhhhhh, now I understand :)

3.2