/ ASME IX WPS range of outside diameter qualified
By
QuocBKA
Date
04-07-2010 14:14
The WPS qualification in accordance with ASME IX I can’t found the range of outside diameter qualified.
So how can I determine the range approval for outside diameter qualified.
Thanks,
Q.V
By
js55
Date
04-07-2010 15:23
You can't find it because it doesn't exist in Section IX.
There is no diameter range for procedure qualification.
By
Mikeqc1
Date
04-07-2010 23:08
Weld metal deposited.
By
3.2 Inspector
Date
04-09-2010 17:48
Kindly explain how weld metal deposited relates to diameter.
Which part of ASME sec 9 did I miss?
3.2
By
Shane Feder
Date
04-10-2010 00:25
3.2,
Take the outside diameter and subtract the inside diameter.
Divide by two and voila - weld metal deposited.
Hope that helps. LOL !!
Cheers,
Shane
By
3.2 Inspector
Date
04-10-2010 01:56
Aaahhhhhhh, now I understand :)
3.2
Topic
American Welding Society Services
/
Certifications
/ ASME IX WPS range of outside diameter qualified
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill