Dear Friends
Appreciate if you could guide me in undestanding the requirements as per AWS D1.1
We have qualified T-Y-K PQR- 6GR Test Coupon( API 5L X52 x API 5L X52 -AWS Group II ) for Mechanical testing.
T-Y-K Joint( used EH36 x EH36-Group II) For Macro Specimens
Question -Is it allowed to use Plate Material (Group II )for Macro-Specimens.OR is it only ALLOWED to use same base material as used for Mechanical Tests Specimens (API 5L X52 )
Appreciate prompt response