I have to test a machine operator on a automatic SAW machine that welds in the 2F position, only T-joints, with the vertical member thickness ranging from 1/4" to 1", but the horizontal member goes from .150 to .375 max. This means that I can't achieve the required size per D1.1 figure 4.37 test, (1/2" min. for the test plates). How do I test the operator?
The operator has passed the test for D1.3, table 4.4, 4.2D (fillet welded T-joint, sheet to supporting member) for a 1/2" vertical member and a 11ga (0.120") horizontal member. But d1.3 is only up to 3/16" thick.
Thank you for the help!