I'm not sure, but I believe AWWA does.
(American Water Works Association)
Best regards - Al
Pickupman
I don't know about building the water tank on the tower although it is fun to watch a good crew.
But I have been called on to make penetrations in the Tower itself for whatever line they need to run.
The only Code referenced for any weld requirements was AWS D1.1.
Marshall
Thanks guys. I'm going to do a little more digging. It's got my curiosity up.
I think Al is correct.
It should be AWWA D100 which is highly connected I believe to D1.1.
I believe my copy is from 1997 and is not current.
Have a Great Day, Brent
We just did a couple of Jobs that were AWWA C206. Most all of AWWA Code refers back to AWS D1.1
Brent and Cactus are correct they are AWWA which refers to AWS D1.1 which is pretty common with any water storage tanks and also steel water lines
Al said it first. Give the credit where it is due!!! LOL!!
Have a Great Day, Brent
I knew someone would know what was going on. Thanks for the replies.