How do you apply the allowable fillet weld undersize criteria (1/16" for 10% of weld length) when measuring intermittent fillet welds? Do you apply it to each individual fillet or the total fillet weld lengths summed up for that weld detail?
You could point out Table 6 (D1.1: 2006)to your welder.
Table 6 (6) Reads: "The size of a fillet weld in any continuous weld may be less than the specified nominal size without correction by the following amounts."