Steve,
What grade of Aluminum wire are you planning to use? There is a shop up the road that has one of those machines and they use a lot of 4043 in a spool gun, but claim they didn't need the spool gun because it ran fine right out of their machine and through the liner. I figure if 4043 runs OK then 5356 should not give any feed problems. I believe they are using .045 dia. wire, but I'm not for sure about the size.
John Wright