ok, we just got back on the qpl list to sell rods to the military
( a cpl years ago ) the other weldor and I had to get qualified to weld to the 10c process."gib 248"
we got the 1/8",3/32", 7/32" and 1/4" 7018 already qpled, now we are working on getting the 5/32" added to the list, however they are gonna
have another weldor do that (one thats not qualified like us)
Me and the other guy really think that this would be wrong, I'm just triing to make sure that we don't do something that could jepordise the company losing our qpl....I guess that I must care too much ...lol
p.s."not really too swift on my communications" and i have a hard time splaining myself. lol so any comments would be good...