Need help!
hello guys...our contractor have qualified wps for gtaw/smaw process, P1 to P1,no impact test, qualified thickness 5 to 20 mm. gtaw filer max deposit 8mm, smaw = 12mm max.
welder have been qualified for 2" dia. x 5.5mm in this wps. can this welder do production joint using the wps but only GTAW process to complete the joint, without exceeding max. deposit qualified for gtaw?