Hao,
You cannot put them in any group - if they are not shown in AWS D1.1 they are classed as "Unlisted" or "Unassigned" (one is AWS and one is ASME but I do not have time to check).
Regardless of which terminology is correct you cannot use that steel for AWS work without qualifying the welding procedures,
Regards,
Shane