Do you have an example? Thickness of butted materials and groove configuration?
Because I would think that joint configuration may dictate a minimum distance just due to geometry. I'm not aware of any such language in the AWS D1.1, AISC Structural Manual or in the Code of Standard Practice that spells out a min. distance per se'.