Dont have my code with me.  Can somebody look and see what group(s) the following 2 materials fall into?
API 5L X70
ASTM A572 G50

Both materials will be 3/16" thick

Thanks for the assist
FAS
Parent - By TimGary (****) Date 07-11-2013 16:34
AWS D1.1:2010, Table 3.1 for Prequalified materials lists A572 Gr50 as a Group II material. API 5L X70 is unlisted in this table.

AWS B2.1 2009 lists both materials as M#1, Group 3
Parent - By jwright650 (*****) Date 07-11-2013 16:34
You didn't say, I'm assuming AWS D1.1 Table 3.1

API 5L X70 - not listed, highest grade I see for API 5L is X52 in Group II
ASTM A572 G50 - Group II

EDIT:
whoops Tim beat me to it.........
Parent - By fschweighardt (***) Date 07-11-2013 17:16
Forgot to say D1.1 2010, not sure what edition my customer is on, but that's what I remembered, X70 as unlisted

Will have to see if my guy is set up on B2.1