Okay, try thinking WAY outside the box here.
1) As John said, 2015 D1.1?? It isn't out yet. Won't be until about October, 2015.
2) Look up at the top of the form: on the left it specifies D1.1 2015; So, I went on line to the downloadable forms to see if they were already out, NOPE. All still based upon the 2010. So where did they get said forms?
![eek :eek:](/f2/epx.png)
3) Then, go over to the right hand side, Annex 'H'?? Forms have been in 'N' for quite some time and 'H' has to do with UT Calibration. ???
4) Not to mention all the other items you guys named, polarity, gas shielding, Short Circuit for Prequalified, etc.
5) Can't spell: THUR ?? (Maybe it is only good on a Thursday?) How about THRU though really THROUGH
6) Travel Speed: '0 - 12"' Really???
I smell a major fraud. I would cry foul big time.