Ok, going to be quick but I have a dilemma. I've been looking thru the code trying to see if there is anything that addresses access to weld areas or welds.
Ok, I know you submarine guys and pipe guys welding thru the gap on the pipe will be laughing but here is my issue. A giant nut 1/4" or less off of a large plate, beveled at 45 degrees for a CJP weld. The nut cannot be removed. To the right of this nut, another nut, about two inches between them. The weld joint is 6 inches long, process, SMAW. Material 1" thick so large bevel height to fill in. Putting the rod in to weld it properly, laughable. Cleaning the weld, hilarious. Improper rod angle galore and the desktop pilot after looking at pictures says, "no issues here". One nut on another plate is smack in the middle of this 6" area to be welded and the nuts are 3-3/8".
I along with the PM are trying to justify our complaints with some sort of documentation. The only thing I have found so far is 5.17.1, AWS D1.1, 2004. The other little tidbit, UT and MT inspections. Told the guy I might as well leave my hood in the truck. I know there are tight spots, have dealt with them many times before but these are in the realm of ridiculous. Ok, I'll attach a picture of one that needs to be repaired for a crack. Crack runs all the way across the weld, very deep. I told them I could give it a go but could not guarantee that it would be picture perfect. I guess I'm also trying to make sure I'm not being a priss!! LOL!!
Weld needs to be built up the 45, brought out flush and a 1/2" reinforcing weld put on. I think I'm having a problem understanding how to bring it out flush with the nut against the weld joint.......