Good morning everyone,
This is the first time i post here. Proud to be part of this welded community.
![grin :grin:](/f2/epx.png)
.
So here comes my problem.
I have to do a welding procedure for CJP 70 mm Round Bar and i have at my disposition the following process : GTAW,SMAW, FCAW .
Material is : S355
type of Joint : Round Bar to Round Bar ( Butt )
Code : AWS D1.1 & BV rules
My question is regarding the Bevel, what kind of Bevel do you suggest for this kind of job ?
Regards