DEAR EXPERTS,
As per AWS D1.1,
1. PIPES LESS THAN 60 DIA AND 3MM HOW TO QUALIFY?
THANKS
By
Lawrence
Date
11-07-2016 13:00
3MM is about 0.118 inches
The minimum base metal thickness for the D1.1 code is 0.125
This fact makes it a possibility that your "Engineer" might want to explore a different specification.
Are you looking for procedure qualification? or performance qualification or both?
This question needs to be presented to your responsible engineer.
By
sharvansiva
Date
11-08-2016 07:28
PROCEDURE QUALIFICATION FOR DIA32.80MM AND THICK 2.3MM
By
Lawrence
Date
11-08-2016 12:52
I think we may have some difficulty understanding each other so far... But not a problem.
Tell us a little more about the pipes and their intended use.
Are these pipes structural, or will they be carrying something?
By
sharvansiva
Date
11-17-2016 08:04
[
http://files.engineering.com/getfile.aspx?folder=e321596d-55e3-45c3-b9e4-56b08603fb9f&file=WPS_DOUBT.jpg%5d%5b%5d
Topic
Welding Industry
/
Inspection & Qualification
/ WPS THICKNESS LESS THAN 3 PIPES
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill