partha_pghosh
Date
11-26-2017 07:43
Required help on the below mentioned points:
1. AWS reference required for the Bunker to Hopper Plate Welding joint at 120 degree
2. Is Butt Weld possible ?
Please refer the attached picture for detail.
Thanks
Partha
Attachment:
1.jpeg
(54k)
By
803056
Date
11-27-2017 02:52
Would this make sense?
Al
Attachment:
MiscBunker26-Nov-2017Model1.pdf
(16k)
By
partha_pghosh
Date
11-28-2017 14:36
Thanks for your response.
What will be the AWS reference for such Bunker to Hopper Plate Welding joint.
Warm Regards
Partha
By
803056
Date
11-29-2017 01:32
AWS D1.1 prequalified groove details and fillet weld details.
Al
Topic
Welding Industry
/
Technical Discussions
/ Bunker to Hopper Plate Welding Joint
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill