- - By partha_pghosh Date 11-26-2017 07:43
Required help on the below mentioned points:

1. AWS reference required for the Bunker to Hopper Plate Welding joint at 120 degree
2. Is Butt Weld possible ?

Please refer the attached picture for detail.

Thanks

Partha
Attachment: 1.jpeg (54k)
Parent - - By 803056 (*****) Date 11-27-2017 02:52
Would this make sense?

Al
Parent - - By partha_pghosh Date 11-28-2017 14:36
Thanks for your response.

What will be the AWS reference for such Bunker to Hopper Plate Welding joint.

Warm Regards

Partha
Parent - By 803056 (*****) Date 11-29-2017 01:32
AWS D1.1 prequalified groove details and fillet weld details.

Al