We had a problem with clad material weldments- the pipeline service for sour gas; hi H2S and CO2. Here's the description:
1. Cald pipe= CS API 5L
2. Cladding with: SS316
3. Welding rod: SS309
Please your inputs: is there risk of dissimilar welding material with the other pipe materials? I.e. there will be a PWC case (preferential weld corrosion) or what would be a cause(s) that might lead to a leak/crack at the welding joint?
Appreciate your inputs and experiences sharing. Thank you in advance
By Israr
Date 10-09-2018 15:50
*1. Mother pipe: CS API 5L
I also want or need your knowledge and experiences with clad material
This thread is rally rather dated. Start a new thread and clearly state your question and provide details of the application and applicable code.
I know starting a new thread can be painful with this site. Been there, so I feel the pain.
Al
Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill