Hello Everyone
I would like to ask you regarding the structure reinforcing pad it is required or not? And the reinforcing pad must be with vent hole and which dimension?!
By
Jim Hughes
Date
10-15-2019 20:49
Need a ton more information, i.e. what code, (AWS D1.1, D1.5 or ?) Give some detail about what size beam or structural component you are building?
By
Ayoub11
Date
10-16-2019 15:50
it is a IPN 300 for a monorail and the total lenght is 30 meter so we have 2 splices in Z format
By
Jim Hughes
Date
10-16-2019 18:02
Edited
10-16-2019 18:37
Need more info. Do you have pictures or drawings? Is this in the US?
Topic
Welding Industry
/
Technical Discussions
/ Structure splice reinforcing pad vent hole
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill