- - By Ayoub11 Date 10-15-2019 14:01
Hello Everyone
I would like to ask you regarding the structure reinforcing pad it is required or not? And the reinforcing pad must be with vent hole and which dimension?!
Parent - - By Jim Hughes (***) Date 10-15-2019 20:49
Need a ton more information, i.e. what code, (AWS D1.1, D1.5 or ?) Give some detail about what size beam or structural component you are building?
Parent - - By Ayoub11 Date 10-16-2019 15:50
it is a IPN 300 for a monorail and the total lenght is 30 meter so we have 2 splices in Z format
Parent - By Jim Hughes (***) Date 10-16-2019 18:02 Edited 10-16-2019 18:37
Need more info. Do you have pictures or drawings? Is this in the US?