Dear all
I am asking about posibility of occuring corrosion between two diffrent grades of steel when welding to gether
eg: A106 grB with api 5l gr x52
Thanks in advance for your help.
By
803056
Date
02-02-2020 00:58
It depends on the environment.
I've seen cases where the HAZ looked like it was removed by a hacksaw, while the weld bead face looked like it was welded the day before yesterday.
Al
By
Amr Elsayed
Date
02-02-2020 08:33
Thanks for reply AL, i am asking if this is mentioned in any code or specs.
By
803056
Date
02-02-2020 14:47
Most welding standard don't address corrosion. The designer has to take that into consideration using a different reference standard. NACE provided a lot of information with regards to corrosion.
Al
Topic
Welding Industry
/
Technical Discussions
/ CS Corrosion
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill