- - By Amr Elsayed Date 02-01-2020 19:39
Dear all
I am asking about posibility of occuring  corrosion between two diffrent grades of steel when welding to gether

eg: A106 grB with  api 5l gr x52

Thanks in advance for your help.    :smile:
Parent - - By 803056 (*****) Date 02-02-2020 00:58
It depends on the environment.

I've seen cases where the HAZ looked like it was removed by a hacksaw, while the weld bead face looked like it was welded the day before yesterday.

Al
Parent - - By Amr Elsayed Date 02-02-2020 08:33
Thanks for reply AL,  i am asking if this is mentioned in any code or specs.
Parent - By 803056 (*****) Date 02-02-2020 14:47
Most welding standard don't address corrosion. The designer has to take that into consideration using a different reference standard. NACE provided a lot of information with regards to corrosion.