- - By bmaas1 (***) Date 10-14-2005 17:20
At risk of sounding dumb can anybody give me a simple procedure for conducting the pretension verification test? I believe I remember exactly how to do it but it has been a long time. No rotational capacity test.

Regards,

Brian
Parent - - By QCCWI (***) Date 10-14-2005 17:41
http://www.boltcouncil.org/2004%20RCSC%20Specification.pdf

OK assemble the bolt nut and washer on the Skidmore tighten it to a snug tight condition(a normal man pulling on a spud wrench or a few impacts with an air wrench).After you get it snug tight mark the head of the boltand nut. Then put a mark on the plate that shows how far you must turn the nut. How far you have to turn the nut depends on the length of the bolt.That part is on the chart in the RCSC book at the link above on page 48( Adobe Acrobat says it is page 60). When you have turned the nut the required distance the Skidmore gauge should read above the required Kips.
Parent - - By bmaas1 (***) Date 10-14-2005 18:07
Thank you. That is pretty much how I remember it.

Brian
Parent - By jwright650 (*****) Date 10-14-2005 19:47
Get some TC Bolts, they are a "snap" to verify in a Skidmore. :)
John Wright

edit: Brian do you have a copy of the structural bolting handbook by SSTC? That is a must have, it has all of the procedures written out for you. All the charts are included for all sizes and strength bolts.
If I remember it is only $10 bucks or so.

http://www.steelstructures.com
Up Topic Welding Industry / General Welding Discussion / Skidmore-Pretension Verification, AISC

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill