Anybody could give me parameters for Spray transfer MIG for
ER CuAl-A2 1,2mm diameter, using Argon ?
Thank you
By
Lawrence
Date
11-27-2005 01:20
Here ya go Goose
http://www.crownalloys.com/page36.pdf
Some folks say U groove rollers and teflon liners also improve GMAW performance of your alloy.
By
Geese_howard
Date
11-27-2005 18:00
I need wire feed speed and stickout also, but thanks anyway
respect to the teflon liner, i dont think is necesary, CuAl-A2 its hard enough for normal liners
By
Lawrence
Date
11-28-2005 05:00
175-275 IPM depending on fillet size required will approximatly corespond with the amperage values you were given.
Stickout between about 3/4 inch (contact tube should be recessed behind nozzle end at least 3/8 inch.
Start with 28 volts.. If your still short circuiting just increase voltage.
If arc length is greater than 1/8 inch reduce voltage 1/2 volt at a time until a nice short arc is achieved.
Topic
Welding Industry
/
Technical Discussions
/ CuAl-A2 spray transfer
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill