D1.5 only lists AASHTO M270 (ASTM A709 steels) so D1.5 will not cover you. If D1.5 is the specified code, you would need to discuss the matter with the engineer for a suitable alternate code. My guess is ASME might apply, but I defer that to those who use ASME.