- - By hogan (****) Date 03-24-2006 21:28
we are welding a 7"x7" tube steel to a 1/4" plate. the detail calls for 1/8" flare bevel weld with a 1/8" fillet on top of flare bevel. can these two welds be made in one pass, or are two passes required? working to aws d1.1
Parent - By medicinehawk (**) Date 03-25-2006 22:47
What process are you planning to use???
If you were to use SMAW, and made your tacks with 3/32"-7018, then I would think you could get a 1/8" fillet weld on the joint design you specified with one pass of 1/8" 7018.
If you are using GMAW say a 70-bare wire, then it would certainly be obtainable with one pass as well.
Parent - By vonash (**) Date 03-27-2006 00:16
I believe your WPS will specify multipass weld.