I will be using the D1.1 code. I would like to have a procedure which has already been qualified using the 3/8 A36 plate with a galvanized coating. According to Section 4, (Fig. 4.32) a Fillet Weld Root Bend Test can be given to certify a welder or welding operator. I do have a WPS for a welding test using 1/2 inch galvanized plate set up in a Tee Joint for the fillet break test. According to section 4, Table 4.10 Fillet Option 1(Fig. 4.36) has to have one fillet break and one macro-etch. I would have to send this off to be tested and at $150.00 each, in order to certify 70 welders this could get costly. Our facility has a saw and a bender, so if I could give the test on 3/8 plate, I could cut it and bend it here. Thanks, Brian