When determining the maximum convexity of fillet welds, the code states in part, "except for outside welds at corner joints". A corner joint would use a fillet weld and if the "other" side is welded, that would really be a butt joint.
Is this reference to the butt weld of the other side or possibly the ends?
Can some one explain what is meant by the term "outside welds"?