7010 exists for the purpose of welding pipe in downhill mode.
The new hippy runs very nice I think. The last two jobs I've had were mainline construction, all hippy, 100% X-ray, and we completed both jobs (14 weeks worth) with a 0% repair rate..
JTMcC.