Gentlemen, I'm asking for your help in double checking me on a Prequalified WPS that I need to write for one of our field superintendents.
He wants to use E7024 SMAW filler rod for fillet welds in the horzontal position out in the field on a structural building, I'm not sure exactly what parts are being joined. These are not-low hydrogen rods. I find it odd that he wants to change to a rod we don't usually use, thus we don't have a WPS on file.
As I read D1.1 (06), pg57, section 3.3 Base Metal /Filler Metal Combinations; They can weld "Any steel to itself or any steel to another in the same group". Thus SMAW E70XX is allowed for group I only to group I, and the relationship would be matching.
But due to this rod is not a low hydrogen rod, it can NOT be used to weld "Any steel in one group to any steel in another."
Basically what I am trying to confirm is that the Table 3.1, Pre-qualified Base Metal-Filler Metal Combinations, is that a Group I material may be welded to itself w/ SMAW E70XX (in my case E7024), but it can Not be used to weld Group II material because it is not listed in Group II Filler Metal Requirments.