Oh I'm sure there is some research out there dealing with heavier inert gases. And my guess would be that chemically, as inerts, they would respond as Argon does. But considering that, as my guess would have it, they are probably way more expensive, why bother?
I might go the other way. Try Neon. It would come at a more resonable price and you could save money on shop lighting.