if it's to D1.1, to my knowledge no. there are req's if in a standard t-joint you have a root opening you have to upsize your fillet weld accordingly, (up to a certain limit). as far as a beveled joint prep, it could be something that your weld engineer deems necessary for a particular circumstance.