- - By EVWELDER (**) Date 01-08-2008 18:11
Is there a standard practice for beveling steel in general on fillet welds example what thickness do you need to start beveling material 3/16" 1/4" ?
Parent - - By jwright650 (*****) Date 01-08-2008 18:43
If fillet welds are called out on the drawing, why would you want to bevel?...just curious.
Parent - By David Lee (*) Date 01-08-2008 18:47
I dont think the norm is to bevel plates etc for fillet weld's
Parent - - By mountainman (***) Date 01-08-2008 18:46
if it's to D1.1, to my knowledge no. there are req's if in a standard t-joint you have a root opening you have to upsize your fillet weld accordingly, (up to a certain limit). as far as a beveled joint prep, it could be something that your weld engineer deems necessary for a particular circumstance.

JJ
Parent - By jwright650 (*****) Date 01-08-2008 18:51
When you start preparing the material, you are getting over into partial pentration groove welds and it is no longer considered a fillet weld.