/ 46100 ARMOR PLATE WELDING PROCEDURE QUESTIONS
By
josephd
Date
02-15-2008 17:11
Does anyone have experience with welding this material? Type of electrode,process, preheat etc. We have a supplier with several small cracks. I suspect lack of preheat.
By
Stephan
Date
02-16-2008 18:36
josephd,
I have remembered, there was a discussion at welding similar materials initiated by Milton at that time, please see also under:
http://www.aws.org/cgi-bin/mwf/topic_show.pl?pid=67903#pid67903
Perhaps you might find some usable information therein.
Best,
Stephan
By
Jim12
Date
03-03-2008 03:42
I FOUND THIS ON THE WEB. GO TO PAGE 104 APPENDIX B
https://aais.ria.army.mil/aais/Padds_web/W52H0908R0048/attach_exhib/att2.pdf
By
chall
Date
03-03-2008 12:55
Nice post. Thanks for putting it up.
Charles
Topic
Welding Industry
/
Metallurgy
/ 46100 ARMOR PLATE WELDING PROCEDURE QUESTIONS
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill