Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Metallurgy / 46100 ARMOR PLATE WELDING PROCEDURE QUESTIONS
- - By josephd (*) Date 02-15-2008 17:11
Does anyone have experience with welding this material? Type of electrode,process,  preheat etc. We have a supplier with several small cracks. I suspect lack of preheat.
Parent - By Stephan (***) Date 02-16-2008 18:36
josephd,

I have remembered, there was a discussion at welding similar materials initiated by Milton at that time, please see also under:

http://www.aws.org/cgi-bin/mwf/topic_show.pl?pid=67903#pid67903

Perhaps you might find some usable information therein.

Best,
Stephan
Parent - - By Jim12 (**) Date 03-03-2008 03:42
I FOUND THIS ON THE WEB. GO TO PAGE 104 APPENDIX B

https://aais.ria.army.mil/aais/Padds_web/W52H0908R0048/attach_exhib/att2.pdf
Parent - By chall (***) Date 03-03-2008 12:55
Nice post.  Thanks for putting it up.