Hi,
I have an application with the foll. specs:
-92 inch ID vessel weldment
-0.25 inch thickness
-0.5 inch thick and 5.375 inch wide flange on either side
I am planning to weld 8 equally spaces stiffeners (3/16th thickness) around the OD (flange to flange).
What welds should I call out for the stiffeners?
The height of the stiffeners is 64 inch flange to flange.
Do I weld it only to the OD of the pressure vessel (intermittent fillet, 2 inch with 4 inch pitch) or
do I call out a weld symbol for welding to the flange as well?
Thanks!