That's what I get for shooting from the hip. You're right, if the base metal is 304L, the filler metal should most likely match the low carbon of the base metal to prevent sensitization if it will be used in a wetted environment and chlorides or other halide ions are expected.
You can use the chemical analysis published by the manufacturer to determine the A number.
Best regards - Al