- - By haonn Date 03-12-2013 06:30
I am trying to figure out a way to make WPS for CSN SN400B, 400C as AWS D1.1
But i am not sure that we can put these materials in which group?
If any help, very anticipate!

Thanks,
HAO
Parent - - By haonn Date 03-15-2013 04:57
Can anyone help me/ give me any advice what to do?

Highly anticipated.
Parent - - By Shane Feder (****) Date 03-15-2013 15:16
Hao,
You cannot put them in any group - if they are not shown in AWS D1.1 they are classed as "Unlisted" or "Unassigned" (one is AWS and one is ASME but I do not have time to check).
Regardless of which terminology is correct you cannot use that steel for AWS work without qualifying the welding procedures,
Regards,
Shane
Parent - By haonn Date 03-21-2013 04:07
Many thanks, Shane