- - By Baraneedharan Date 05-17-2017 18:41
1. Check list before welding of clad materials
2. Among the check list most important to be checked before welding
Parent - By 803056 (*****) Date 05-18-2017 11:54
So, what's the question?

Al
- - By Israr Date 10-09-2018 15:49
Dear Colleagues,
We need your knowledge and experiences sharing;

We had a problem with clad material weldments- the pipeline service for sour gas; hi H2S and CO2. Here's the description:
1. Cald pipe= CS API 5L
2. Cladding with: SS316
3. Welding rod: SS309

Please your inputs: is there risk of dissimilar welding material with the other pipe materials? I.e. there will be a PWC case (preferential weld corrosion) or what would be a cause(s) that might lead to a leak/crack at the welding joint?

Appreciate your inputs and experiences sharing. Thank you in advance
Parent - By Israr Date 10-09-2018 15:50
*1. Mother pipe: CS API 5L
- - By mariagarcia (*) Date 05-23-2019 12:18
I also want or  need your knowledge and experiences with clad material
Parent - By 803056 (*****) Date 05-23-2019 14:31
This thread is rally rather dated. Start a new thread and clearly state your question and provide details of the application and applicable code.

I know starting a new thread can be painful with this site. Been there, so I feel the pain.

Al
Up Topic Welding Industry / Welding Fundamentals / Welding of clad materials

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill