what are you referring to
Welderdan, to me that looks like a pit in the pipe, not a grinder mark, correct if i'm wrong.
this is jrw159, and It does look like a pit, but why is it shiny while the numerous others that appear to be equal are not.
It might be nothing, but from my standpoint any time you see something like that it warrants a closer look.
And I am probably way off base as to what Kix is refering too.
Dad gummm, I wish he would give it up! :-)
Those stringer bead brushes can polish those pits pretty good.
welderdan, I think that pretty good work good even shape and so on. clean edges no undercuts.
I agree, but with a wire brush attachment you will leave a bigger footprint, or shiny spot.
And yes by apearances the welds look good. :-)
jrw159
thought for the day, no matter how you try to polish a turd, its still a turd. those welds ain't turds
i agree with ya man look pretty slick to me

;-) got cha
Kix,
OK partner, you have me wondering.
I see one spot on center right of one pic that looks like a possible grinder hit or ground down arc strike, but I can not be positive.
Tell us my friend, what it is you see. :-)
I ask this in the most respectful way, as I hold your opinion/interpretation at a high level.
John
EDIT: Unless you mean are they going to wrap, jeep, run pigs, and backfill, with compaction, cleanup and reseed per specs. Because if so, you are right, they are far from done. :-)

Looks like soap-stone to me. Then again, I just got back from Hooters and my vision is skewed.
well,,,that looks descent and all but its not somethin id leave on a piece of pipe. the first thing i see is that damn start. what happened there dude. its kinda small on my computer but from what i can see,,,if you wanna make a slick ass cap,,,slow down and long arc a little more with that 70+,,,itll look better. and if thats some of your best work we need to meet up so i can adjust your machine. but dont get me wrong,,,i see way worse all day long and very few times find a good lookin cap. let me see if i can get these pics off this phone and ill show u a slick ass cap