- - By aliabdou93 Date 08-25-2019 18:27
can i use 6010 for the root & 6013 for the fill/cap ?
Parent - - By 803056 (*****) Date 08-26-2019 01:05
What was qualified. They are different F numbers, so a different PQR may be needed if the current WPS doesn't permit it.

Then again, if the governing code is the Farm Code, it is perfectly fine until it breaks.

Al
Parent - - By aliabdou93 Date 08-26-2019 08:00
it's qualified yes but they aren't the same F number , so there is a problem ?
Parent - - By SWN1158 (***) Date 08-26-2019 13:57
Do the project specs limit you to E70xx ?
Parent - By aliabdou93 Date 08-27-2019 06:01
NO
Parent - - By 803056 (*****) Date 08-26-2019 15:49
Read my response.

Al
Parent - By Shane Feder (****) Date 08-27-2019 10:44