/ cellulosic and rutile
By
aliabdou93
Date
08-25-2019 18:27
can i use 6010 for the root & 6013 for the fill/cap ?
By
803056
Date
08-26-2019 01:05
What was qualified. They are different F numbers, so a different PQR may be needed if the current WPS doesn't permit it.
Then again, if the governing code is the Farm Code, it is perfectly fine until it breaks.
Al
By
aliabdou93
Date
08-26-2019 08:00
it's qualified yes but they aren't the same F number , so there is a problem ?
By
SWN1158
Date
08-26-2019 13:57
Do the project specs limit you to E70xx ?
By
aliabdou93
Date
08-27-2019 06:01
NO
By
803056
Date
08-26-2019 15:49
Read my response.
Al
By
Shane Feder
Date
08-27-2019 10:44
Yes, there is a problem.
Topic
Welding Industry
/
Technical Discussions
/ cellulosic and rutile
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill