as too why
it shows you can really weld with SMAW
many, many decades ago
that was the welding test for Los Angeles city structural steel test cert
1" all 4 positions ie: flat, horizontal, vertical, and overhead
then you had the written test
the old days....when that was the gold standard
they laughed at AWS cert 3/4" test plates, no written test
![eek :eek:](/f2/epx.png)
as far as tips for the root pass
whip it, use the z type motion
DC+ 100-120 amps for 1/8" electrode
at least works for me
hope this helps
sincerely,
Kent