Info
For postings/queries strictly concerning Inspection
Topic
User
Posts
Last Post
UT and Current 31.3
js55
4
08-06-2008 11:13
Longitudinal acceptance criteria for distorted spools
Richman
7
08-04-2008 21:08
Why did this fail Charpy V-notch impact
Mikeqc1
21
08-04-2008 10:17
Why did this fail Charpy V-notch impact
Mikeqc1
1
07-30-2008 15:58
pipeline cap height
Yardbird
24
07-29-2008 16:43
Stud Welding Symbol
Razor20
3
07-29-2008 16:02
Weldin travel speed
rafael Angarita
9
07-26-2008 02:18
Purchase order vs Spec.
Mikeqc1
8
07-24-2008 13:50
What can i expect with my experience ?
chang
10
07-24-2008 01:41
weld etching chemicals
Strongarc
5
07-23-2008 20:09
Acceptance criteria for distorted spool
Richman
4
07-23-2008 19:53
Inspection ethics
Pipeslayer
15
07-22-2008 19:27
UT of plug welds
hogan
3
07-22-2008 15:57
RT - ASME Spot Examination
chang
7
07-20-2008 06:25
UT Question: stainless versus carbon steeel
Bill M
3
07-17-2008 17:53
CJP or PJP?
jrw159
10
07-17-2008 15:55
RT interpretation on ASME B31.1
swsweld
20
07-14-2008 22:13
Gamma v X-ray
Shane Feder
30
07-14-2008 21:52
Defusible hydrogen content testing
jrw159
9
07-11-2008 20:16
Welder Qualified ASME IX
DAYANARA
7
07-11-2008 18:30
Arrestallamas en Tks de Petroleo /Flame arresters on OIl Tks
JCaprarulo
1
07-11-2008 17:51
CWI en Monterrey
LuciaLopez
24
07-11-2008 00:14
Visual inspection forms
jrw159
9
07-10-2008 20:13
what do you think
raptor34
34
07-10-2008 16:15
how much authority
strat
10
07-10-2008 14:46
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill