used in high-temperature applications are becoming more complex to achieve the creep strength and corrosion resistance. A range of low-alloy, high-strength, and austenitic materials are required depending on the application. What choices does the engineer have once the weldability window for high-temperature steels is cut in half? Topics to be covered include weldability of P91 steel, welding dissimilar metals, postweld heat treating, new welding consumables, and managing weld cracking. AWS 18th Annual Aluminum Conference. Sept. 22–24. San Diego, Calif. A panel of distinguished aluminum-industry experts will survey the state of the art in welding technology and practice. Attendees will network informally with the speakers and visit an exhibition showcasing the latest products and services offered by aluminum industry providers. ITSA Thermal Spray for Oil and Gas Conference and Exhibits. October TBA, Houston, Tex. This two-day event will explore the latest technologies and applications for thermal spraying in the oil and gas exploration, production, refining, and distribution industries. FABTECH 2015. Nov. 9–12. McCormick Place, Chicago, Ill. This exhibition is the largest event in North America dedicated to showcasing welding, metal forming, fabricating, tube and pipe equipment and services plus myriad manufacturing and related technologies. Attend the American Welding Society’s business meetings, awards-presentations, educational programs, and welding contests. (800/305) 443- 9353, ext. 264; www.fabtechexpo.com. Like us on facebook Weld T Test Stand The Weld Test Stand allows secure and positioning of pipe or plate test assemblies. To demonstrate versatility our advertisement shows (3) plate fixtures, (1) pipe fixture & (4) adjustable overarms. Stand* comes complete with Base, Mast, Tool Tray, (1) Overarm, and Top Brace Pipe and plate holding fixtures sold separately and can be used in any bench vise Plate fixture: 1-1/2” thick max. capacity in any position Pipe fixture: 1. 25” thick max. capacity in any position Pipe fixture has gas purging capabilities. *Model# WTS-ASSY WTS-P256G .com For info, go to www.aws.org/adindex APRIL 2015 / WELDING JOURNAL 79 SERIOUS AIR for SERIOUS PLACES NEW! The ideal solution for employee comfort and productivity! TRIANGLE ENGINEERING, INC. WTS-MAST (INCL) WTS-PL 6 Industrial Way, Hanover, MA 02339-2425 www.trieng.com WTS-TB (INCL) TRIANG ENGINE allows for quick, e clamping WTS-OVARM/1 (INCL) WTS-TT (INCL) Tool WTS-TBL-ASSY WTS-BASE (INCL) Hanove trie For info, go to www.aws.org/adindex For info, go to www.aws.org/adindex
Welding Journal | April 2015
To see the actual publication please follow the link above